Nickel Alloy 200 /201

Nickel Alloy 200 /201

Nickel 200 (UNS N02200) (EN 2.4066)
Nickel 201 (UNS N02201) (EN 2.4068 LC-Ni 99.2)

Nickel 200 and  Nickel 201 are unalloyed nickel with a nickel concentration of at least 99.2%. Nickel 201 is the low carbon version of  Nickel 200.

They are characterized by:

  • Excellent resistance in alkaline media.
  • High ductility in a wide temperature range.
  • Ferromagnetism.
  • High electrical and thermal conductivity.

Chemical Composition

Nickel 200

Nickel 201

Physical Composition

Nickel 200

Nickel 201

Designations & Standards

Applications
  • Applications include chemical shippingdrums, electrical and electronic parts, aerospace and missile components