Hastelloy C276 Seamless Pipe, ASTM B619 Alloy C276 Welded Pipes, Hastelloy UNS N06022 Pipes, Alloy 2.4602 Seamless Pipes, Hastelloy C276 Pipes Stockist in Mumbai, India
MV Super Alloys is a worldwide Importer and Stockist of Hastelloy C276 Pipes. We deal with quality products and excellent quality raw materials to make long-life products. Get in touch to know more about us.
We offer an extended range of Hastelloy pipes and Hastelloy pipe fittings in various standards, including the following: Hastelloy C276, Hastelloy c276, Hastelloy C276, etc. The forms available to us are custom-made dimensions.
Features of the pipes
Using lower carbon version alloys, Hastelloy C276 Pipes are used in various environments. Hastelloy C276 pipes are nickel-chromium alloy known as versatile corrosion resistance alloy because of lower carbon composition.
Apart, this grade shows good fabricability and doesn’t require heat treatment. Hastelloy C276 is a nickel-chromium-molybdenum-tungsten alloy used under localized corrosion as well as a uniform corrosion-resistant environment. Hastelloy C276 pipes are used across chemical industries and can be effective because of exceptional resistance properties in those environments.
Hastelloy C276 alloy pipes are used against cupric oxides, usually ferric and cupric chlorides, hot heat-treating media, and more to provide enough resistance in all of those environments. Hastelloy c276 also offers excellent stress corrosion cracking, all thanks to their properties.
We possess a stringent quality of tests such as mechanical tests, macro and micro tests, flaring tests, hardness tests, chemical tests like automated tests, etc., to ensure the best quality and long service life of these pipes.
Hastelloy C276 Pipe Stockist, Hastelloy C276 Welded Pipe, ASME SB 622 Alloy C276 Seamless Pipes, Hastelloy Alloy C276 Seamless Pipes, Alloy C276 ERW Pipe, Hastelloy C276 Pipes Importer in India
Hastelloy C276 Round Pipes, Nickel Alloy C276 Pipes, C276 Alloy Seamless Pipes traders, Hastelloy C276 Pipes at Best Price, Hastelloy DIN 2.4602 Pipes, Alloy C276 Seamless Pipes Stockist in India
ASME SB622 Alloy C276 Pipes Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS | JIS | GOST | EN | OR |
| Hastelloy C276 | 2.4610 | N06455 | – | – | – | – |
| Hastelloy C276 | 2.4602 | N06022 | NW 6022 | – | NiCr21Mo14W | – |
| Hastelloy C276 | 2.4819 | N10276 | NW 0276 | ХН65МВУ | NiMo16Cr15W | ЭП760 |
Hastelloy C276 Pipe Forms in Stock
Hastelloy C276 Seamless Pipes:
- Hastelloy C276 seamless pipes are pipes made from the corrosion-resistant alloy Hastelloy C276 without any welding joints. These pipes are Stockistd through a seamless process, where a solid cylindrical billet of Hastelloy C276 is heated and then stretched to form a seamless tube. The absence of welds in seamless pipes ensures higher strength and corrosion resistance, making them suitable for critical applications in industries such as chemical processing, petrochemical, and oil and gas.
Hastelloy C276 Welded Pipes:
- Hastelloy C276 welded pipes are pipes made from Hastelloy C276 alloy that are joined together using various welding techniques. These pipes are Stockistd by rolling or bending a flat strip or plate of Hastelloy C276 into a cylindrical shape and then welding the longitudinal seam. Welded pipes are available in different sizes and are widely used in applications where cost-effectiveness and less critical environments are essential.
Hastelloy C276 ERW Pipes:
- Hastelloy C276 ERW (Electric Resistance Welded) pipes are a type of welded pipe made from Hastelloy C276 alloy. ERW pipes are created by rolling a flat sheet of Hastelloy C276 into a cylindrical shape and then welding the longitudinal seam using electric resistance. ERW pipes offer excellent dimensional accuracy and are commonly used in applications that require precise tolerances and resistance to corrosive environments.
Stock Size Range and Specifications For Hastelloy C276 Pipe
| Specification | ASTM B622, B619 / ASME SB622, SB619 |
| Dimension Standard | ANSI B36.19M, ANSI B36.10 |
| Outside Diameter | 1.250″ – 6.000″ (30-150mm) |
| Size | 15″NB – 150″NB |
| Wall Range | 0.095″ – 1.000″ (.2.5-25mm) |
| Type | Seamless / ERW / Welded / Fabricated Pipes |
| Form | Round, Square, Rectangular, Oval, Hydraulic Etc |
| Length | Single Random, Double Random & Required Length |
| End | Plain End, Beveled End, Treaded |
| End Protection | Plastic Caps |
| Delivery Condition | Annealed and Pickled, Polished, Bright Annealed, Cold Drawn |
| Inspection, Test Reports | Mill Test Certificates, EN 10204 3.1, Chemical Reports, Mechanical Reports, PMI Test Reports, Visual Inspection Reports, Third Party Inspection Reports, NABL Approved Lab Reports, Destructive Test Report, Non Destructive Test Reports |
| Packing | Packed in Wooden Boxes, Plastic Bags, Steel Strips Bundled, or as per Customers Requests |
| Specials | Sizes and Specifications other than above can be tailored on request |
Chemical Composition of Hastelloy C276 Pipes
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C276 | 0.015 max | 1.0 max | 0.08 max | 0.03 max | 2.0 max | Bal | 14.00-18.00 max | 3.0 max | 14 – 17 | 0.04 max |
| C276 | 0.010 max | 0.50 max | 0.08 max | 0.02 max | 2.50 max | 50.015 min* | 20.00 – 22.50 | 2.00 – 6.00 | 12.50 – 14.50 | 0.02 max |
| C276 | 0.010 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.00 – 17.00 | 0.04 max |
Mechanical Properties of Hastelloy C276 / N06022 / 2.4602 / NW 6022 Pipes
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C276 | 9.2 g/cm3 | 1370 °C (2500 ºF ) | Psi – 1,10,000 , MPa – 760 | Psi – 51000 , MPa – 350 | 40 % |
| Hastelloy C276 | 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000 , MPa – 690 | Psi – 45000 , MPa – 310 | 45 % |
| Hastelloy C276 | 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52,000 , MPa – 355 | 40 % |
WNR 2.4602 Hastelloy Pipe Schedule Chart
Get the Schedule Chart of Hastelloy C276 pipe, from 1/8* Iron Pipe Size to 18* Iron pipe Size Schedule Table, Hastelloy C276 Pipe Stockist in Dubai.
| 1/8″ IPS(.405″O. D.) | 3 1/2″ IPS( 4.000″O. D.) |
| SCH 40, 80 | SCH 10, 40, 80, 160, XXH |
| 1/4″ IPS(.540″O. D.) | 4″ IPS(4.500″O. D.) |
| SCH 10, 40, 80 | SCH 10, 40, 80, 160, XXH |
| 3/8″ IPS(.675″O. D.) | 5″ IPS( 5.563″O. D.) |
| SCH 10, 40, 80 | SCH 10, 40, 80, 160, XXH |
| 1/2″ IPS(.840″O. D.) | 6″ IPS(6.625″O. D.) |
| SCH 5, 10, 40, 80, 160, XXH | SCH 5, 10, 40, 80, 120, 160, XXH |
| 3/4″ IPS(1.050″O. D.) | 8 ” IPS(8.625″O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH 5, 10, 40, 80, 120, 160, XXH |
| 1″ IPS:(1.315′O. D.) | 10″ IPS(10.750″O. D.) |
| SCH 5, 10, 40, 80, 160, XXH | SCH 10, 20, 40, 80 (.500), TRUE 80(.500) |
| 1-1/4″ IPS(1.660″O. D.) | 12″ IPS(12.750″O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH 10, 20, 40(.375), TRUE40(.406), SCH80(.500) |
| 1-1/2″ IPS(1.900″O. D.) | 14″ IPS(14.000″O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH10 (.188), SCH40 (.375) |
| 2″ IPS(2.375″O. D.) | 16″ IPS(16.000″O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH10(.188), SCH40(.375) |
| 2 1/2″ IPS(2.875″O. D.) | 18″ IPS (18.000″O. D.) |
| SCH 10, 40, 80, 160, XXH | SCH-40 (.375) |
| 3″ IPS( 3.500″O. D.) | |
| SCH 5, 10, 40, 80, 160, XXH |
Hastelloy C276 Pipes Application Industries
- Aerospace Industry
- Chemical Industry
- Energy Industry
- Food Processing Industry
- Oil and Gas Industry
- Petrochemical Industry
- Pulp & Paper Industry
- Pharmaceuticals Industry
- Power Plant Industry
People Also Searched for
hastelloy C276 seamless pipe Stockist, hastelloy C276 seamless pipes Stockist in india, alloy C276 pipe price list, hastelloy C276 pipe Stockist in india, seamless hastelloy C276 pipe, hastelloy C276 pipes Stockist in mumbai, hastelloy C276 pipe price list in india, alloy C276 erw pipe Stockist, hastelloy C276 pipe price, astm b622 alloy C276 seamless pipe, weight of hastelloy C276 pipe, cost of C276 hastelloy alloy pipe, hastelloy C276 pipe sizes, nickel alloy hastelloy C276 pipes, hastelloy C276 large diameter pipes, hastelloy C276 welded pipe Stockist, alloy C276 seamless pipe Stockist, hastelloy C276 pipe weight calculator, alloy C276 pipe price per meter, hastelloy C276 pipe weight, hastelloy C276 pipe Stockists in india, asme sb622 hastelloy C276 pipe, hastelloy C276 pipe price list pdf, hastelloy C276 pipe weight chart, hastelloy C276 pipe price per kg in india, alloy C276 seamless nickel pipe, alloy C276 pipe Stockist in mumbai, price of nickel alloy pipe C276.
Product
| Incoloy 825 Pipes & Tubes |
| Incoloy 825 Plates & Sheets |
| Incoloy 825 Flanges |
| Incoloy 825 Filler wire |
| Incoloy 825 Round Bars |
| Incoloy 825 Coils |
| Incoloy 825 Buttweld Fitting |