Hastelloy C276 Round Bars

ASTM B335 C276 Hastelloy Bars, Hastelloy UNS N10665 Round Bar, Hastelloy C276 Square Bar, Hastelloy C276 Flat Bar, ASTM B335 C276 Hastelloy Hex Bar, Hastelloy Alloy C276 Round Bar, C276 Hastelloy Rods, Hastelloy C276 Round Bar Stockist in Mumbai, India.

MV Super Alloys is a steel Importing and Stocking organisation that specialize in a extensive range of steels, specifically Hastelloy C276 fasteners. We are the state in the global and the world’s oldest and biggest providers of fittings, with a long time, a team of particularly certified employees, and more advantageous steel production.

Hastelloy C276 grades are available in diverse sizes and might even be shipped anywhere outside the world. Hastelloy C276 is a nickel-molybdenum alloy with terrific bodily and mechanical houses and terrific corrosion resistance. C276 kind is extra touchy to intense warmness in warmness remedy settings. After welding, this type does not require warmth treatment. This grade is known to tolerate grain-boundary precipitation, which is customary in warmer climates, and the stepped forward fabricability is appropriate for chemical method applications. Hastelloy C22 is a sophisticated variation of alloy C, a nickel-chromium-molybdenum tungsten buttweld becoming with notable weldability and corrosion resistance in localized and uniform corrosive environments. This grade may be utilized in several chemical additives and strong oxidizers together with ferric chlorides and hot contaminated areas, seawater, and numerous different environments. This grade is likewise proof against grain-boundary precipitation, as defined by using the C276 alloy. Hastelloy C22 is normally now not recommended at temperatures exceeding 1250°F because of the formation of dangerous stages at extraordinarily excessive temperatures greater than 1250 stages celsius.

Chemical industries, pharmaceutical gadget, petrochemical industries, oil and gas industries, and many more industries rent Inconel C276 superalloy round bars. We also provide above fasteners in a number of shapes and sizes and different adjustments.

Hastelloy C276 Bright Bar Stockists, Hastelloy Alloy C276 Rods, Hastelloy 2.4610 Round Bars, Hastelloy C276 Cold Finish Round Bar, ASTM B335 Hastelloy C276 Round Bars, Hastelloy C276 Forged Bar Importer in India.

ASTM B335 C276 Hastelloy Round Bar, Hastelloy Alloy C276 Industrial Bars Traders, ASTM B335 Hastelloy C276 Hexagonal Bars, Hastelloy C276 Threaded Bar, ASTM B335 Hastelloy C276 Round Bar at Best Price, Hastelloy C276 Polished Bars Stockist in India.

ASTM B335 Hastelloy C276 Round Bars Equivalent Grades

STANDARD WERKSTOFF NR. UNS JIS GOST EN OR
Hastelloy C4 2.4610 N10665 – – – –
Hastelloy C22 2.4602 N06022 NW 6022 – NiCr21Mo14W –
Hastelloy C276 2.4819 N10276 NW 0276 ХН65МВУ NiMo16Cr15W ЭП760

 

ASTM B335 Hastelloy C276 Bars Forms in Stock

ASTM B335 Hastelloy C276 Round Bar:

ASTM B335 Hastelloy C276 round bar is a cylindrical, stable steel bar made from the corrosion-resistant alloy Hastelloy C276. It is Stocked to fulfill the specifications outlined in ASTM B335, making sure superb and reliable performance. Hastelloy C276 round bars are broadly utilized in various industries, together with chemical processing, marine, and petrochemical, for applications requiring terrific resistance to corrosive environments and excessive temperatures.

ASTM B335 Hastelloy C276 Square Bar:

ASTM B335 Hastelloy C276 rectangular bar is a 4-sided, solid metallic bar with rectangular go-sections, made from Hastelloy C276 alloy. The rectangular form gives additional electricity and tension, making it suitable for applications where square or angular additives are required. Like round bars, rectangular bars are applied in industries that demand super corrosion resistance and mechanical properties.

ASTM B335 Hastelloy C276 Hollow Bar:

ASTM B335 Hastelloy C276 hole bar is a tubular metallic bar with an empty indoors, supplying a lightweight option at the same time as keeping the power and corrosion resistance of Hastelloy C276. Hollow bars are used in applications in which weight loss is essential without compromising overall performance. They discover usage in industries like aerospace, car, and structural engineering.

ASTM B335 Hastelloy C276 Hex Bar:

ASTM B335 Hastelloy C276 hex bar is a six-sided, strong metallic bar with a hexagonal pass-phase. The unique shape gives higher gripping surfaces and is suitable for packages requiring precise rotation or alignment. Hastelloy C276 hex bars are widely used in industries like equipment, fasteners, and valves.

ASTM B335 Hastelloy C276 Bright Bar:

ASTM B335 Hastelloy C276 vibrant bar refers to round bars with a sophisticated surface end, supplying an easy and splendid appearance. Bright bars are used in ornamental applications, in addition to in industries wherein an aesthetically attractive floor is wanted, along with structure and interior layout.

ASTM B335 Hastelloy C276 Forged Bar:

ASTM B335 Hastelloy C276 stable bar is produced via a forging system, which includes shaping the metallic below high stress to decorate its power and grain shape. Forged bars are stated for their more mechanical homes, making them appropriate for vital programs wherein higher energy and durability are required.

Stock Size Range and Specifications For ASTM B335 Hastelloy C276 Round Bar

Specification  EN, DIN, JIS, ASTM, BS, ASME, AISI
Standard Specification  ASTM B574 / ASTM SB574
Size  15NB to 150NB IN
Diameter  3.17mm to 350mm diameter
Length  100 mm to 3000 mm Long & Above
Tolerance  H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients’ requirements
Finish  Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish
Form  Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc
Surface  Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline
Condition  Cold Drawnd Pulished Cold Drawn Centreless Ground & Polished

Chemical Composition of Hastelloy C276 Round Bars

Grade C Mn Si S Co Ni Cr Fe Mo P
C4 0.02 max 1.0 max 0.1 max 0.03 max 1.0 max Bal 1.0 max 2.0 max 26 – 30 0.04 max
C22 0.010 max 0.50 max 0.08 max 0.02 max 2.50 max 50.015 min* 20.00 – 22.50 2.00 – 6.00 12.50 – 14.50 0.02 max
C276 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 max

Mechanical Properties of Hastelloy C276 / N10665 / 2.4610 Round Bars

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C4 9.2 g/cm3 1370 °C (2500 ºF ) Psi – 1,10,000 , MPa – 760 Psi – 51000 , MPa – 350 40 %
Hastelloy C22 8.69 g/cm3 1399 °C (2550 °F) Psi – 1,00,000 , MPa – 690 Psi – 45000 , MPa – 310 45 %
Hastelloy C276 8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %

 

ASTM B335 Hastelloy C276 Bars Application Industries

  • Aerospace Industry
  • Chemical Industry
  • Energy Industry
  • Food Processing Industry
  • Oil and Gas Industry
  • Petrochemical Industry
  • Pulp & Paper Industry
  • Pharmaceuticals Industry
  • Power Plant Industry

People Also Searched for

Werkstoff Nr. 2.4819 Hexagonal Bar Trader, Werkstoff Nr. 2.4819 Half Round Rod Trader, UNS N10276 Polished Bar wholesaler, Alloy C276 Hexagonal Bar Stockist, UNS N10276 Bright Rod wholesaler, Hastelloy C276 Rectangular Bar Stockist, Werkstoff Nr. 2.4819 Half Round Bar Stockist, Hastelloy C276 Bright Rod stockist, Hastelloy C276 Hex Rod retailer, UNS N10276 Threaded Bar retailer, ASME SB574 Bright Rod stockist, Werkstoff Nr. 2.4819 Hot Rolled Rod Trader, Werkstoff Nr. 2.4819 Peeled Bar wholesaler, ASTM B574 Bright Rod Stockist, UNS N10276 Y Shape Bar Stockist, Bright Bar Stockist, Alloy C276 Triangle Bar Stockist, Werkstoff Nr. 2.4602 Hex Bar wholesaler, Werkstoff Nr. 2.4602 Threaded Bar stockist, Polished Rod Stockist, UNS N06022 Square Bar Stockist, Werkstoff Nr. 2.4602 Industrial Rod Stockist, Hot Rolled Rod Trader, ASTM B574 Black Bar wholesaler, Alloy C22 Polished Rod trader, UNS N06022 Round Rod Trader, Alloy C22 Industrial Bar Trader, Black Bar trader, Werkstoff Nr. 2.4602 Hexagonal Bar Trader, Alloy C22 Black Rod Trader, Hex Rod wholesaler, ASTM B574 Polished Bar Trader, Werkstoff Nr. 2.4602 Hex Bar stockiest, Round Bar stockiest, Industrial Bar trader, Hastelloy C22 Hot Rolled Bar retailer, Werkstoff Nr. 2.4819 Half Round Rod Stockist in Malaysia, Werkstoff Nr. 2.4819 Hex Bar Importer in Indonesia, ASME SB574 Industrial Bar trader in Coimbatore, ASTM B574 Threaded Rod wholesaler in Qatar, Triangle Bar Trader in Kolkata, Werkstoff Nr. 2.4819 Hexagonal Rod Trader in Vietnam, Round Rod stockist in Saudi Arabia, ASTM B574 Industrial Bar Importer in Kolkata, Round Rod Importer in India, Triangle Bar Trader in Ahmedabad, Alloy C276 Bright Rod stockist in Singapore, UNS N10276 Triangle Rod stockist in Qatar, Hastelloy C276 Threaded Rod retailer in Saudi Arabia, ASME SB574 Polished Bar Importer in India, ASTM B574 Cold Drawn Rod Trader in Pune, Half Round Bar Trader in Kuwait, Hexagonal Bar wholesaler in Mumbai, ASTM B574 Rectangular Bar retailer in Mumbai

Product
    Inconel 718 Pipes & Tubes
    Inconel 718 Plates & Sheets
    Inconel 718 Flanges
    Inconel 718 Filler wire
    Inconel 718 Round Bars
    Inconel 718 Coils
    Inconel 718 Buttweld Fitting
    Incoloy 825 Pipes & Tubes
     Incoloy 825 Plates & Sheets
    Incoloy 825 Flanges
     Incoloy 825 Filler wire
     Incoloy 825 Round Bars
     Incoloy 825 Coils
     Incoloy 825 Buttweld Fitting
Latest Post
Get A Quote
sales@mvsapl.com