Alloy K500 Seamless Pipe, ASTM B725 Monel K500 Welded Pipes, Monel UNS N04K500 Pipes, Alloy 2.4360 Seamless Pipes, Monel K500 Pipes Stockist in Mumbai, India.
MV Super Alloys is the traditional Stockist and Trader of Monel K500 Pipes locally and worldwide. We feature standard shapes, sizes, dimensions, and even custom-made specifications upon the client’s demands.
Monel K500 pipes are age -hardenable nickel-copper alloy. They have a useful composition of aluminum and titanium that stabilize their properties, such as corrosion resistance and high strength over high-temperature environments. Monel K500 Pipe is the redeveloped version of alloy K500 to improve corrosion resistance and enhance strength.
Monel K500 alloy has advantages such as two times yielding power and up to 3 times tensile strength by comparison to the alloy K500. Monel K500 can perform cold working operations before precipitation hardens. The mechanical properties of Monel K500 are also excellent from subzero temperature up to 480 degrees C.
Monel K500 performs extensively better at environments such as marine and chemical atmospheres including pure water to high oxidized mineral acids. Monel K500 shows non-magnetic properties and, therefore, should be welded to get annealed, then the weldments after that stress relieved before the aging.
Monel K500 alloys pipes are available in various shapes, sizes including 3/8″ to 2-1/2″ diameter, and also available in hot finished aged or anneal aged as per the requirements, that can be used in various industries including oil and gas industries, oil and gas industries, heat generation, petrochemical equipment, chemical processing, and so on.
Monel K500 Seamless Pipes, Monel K500 Pipe Stockist, Monel Alloy K500 Pipes, Alloy K500 Pipes, Monel K500 Welded Pipe, ASME SB 165 Alloy K500 Seamless Pipes Importer in India.
Alloy K500 Seamless Pipes, Monel K500 Seamless Pipes Trader, Monel K500 Round Pipes, Monel K500 Pipes at Best Price, Monel DIN 2.4360 Pipes, Alloy K500 ERW Pipe Stockist in India.
Alloy K500 Pipes Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Monel K500 | 2.4360 | N04K500 | NW 4K500 | NA 13 | МНЖМц 28-2,5-1,5 | NU-30M | NiCu30Fe |
Monel K500 Pipe Forms in Stock
Monel K500 Seamless Pipes:
- Monel K500 seamless pipes are tubular products made from the nickel-copper alloy Monel K500 without any welded seams. They are manufactured using a seamless extrusion process, providing a smooth, continuous surface and uniform dimensions. Monel K500 seamless pipes are known for their excellent resistance to corrosion and high-temperature environments, making them suitable for various applications in marine engineering, chemical processing, and oil and gas industries.
Monel K500 Welded Pipes:
- Monel K500 welded pipes are tubular products made from the Monel K500 alloy through welding processes. The pipes are formed by joining two pieces of Monel K500 plates or coils using welding methods such as electric resistance welding (ERW), electric fusion welding (EFW), or high-frequency induction welding (HFIW). Monel K500 welded pipes are commonly used in applications where ease of fabrication and installation is required.
Monel K500 ERW Pipes:
- Monel K500 ERW pipes are tubular products made from the Monel K500 alloy using the electric resistance welding (ERW) process. In this method, the edges of Monel K500 plates or coils are heated and fused together under pressure to form the pipe. Monel K500 ERW pipes are widely used in various industries due to their excellent resistance to corrosion, high strength, and ease of welding.
Stock Size Range and Specifications For Monel K500 Pipe
| Specification | ASTM B165, B725 / ASME SB165, SB725 |
| Dimension Standard | ANSI B36.19M, ANSI B36.10 |
| Outside Diameter | 1.250″ – 6.000″ (30-150mm) |
| Size | 15″NB – 150″NB |
| Wall Range | 0.095″ – 1.000″ (.2.5-25mm) |
| Type | Seamless / ERW / Welded / Fabricated Pipes |
| Form | Round, Square, Rectangular, Oval, Hydraulic Etc |
| Length | Single Random, Double Random & Required Length |
| End | Plain End, Beveled End, Treaded |
| End Protection | Plastic Caps |
| Delivery Condition | Annealed and Pickled, Polished, Bright Annealed, Cold Drawn |
| Inspection, Test Reports | Mill Test Certificates, EN 10204 3.1, Chemical Reports, Mechanical Reports, PMI Test Reports, Visual Inspection Reports, Third Party Inspection Reports, NABL Approved Lab Reports, Destructive Test Report, Non Destructive Test Reports |
| Packing | Packed in Wooden Boxes, Plastic Bags, Steel Strips Bundled, or as per Customers Requests |
| Specials | Sizes and Specifications other than above can be manufactured on request |
Chemical Composition of Monel K500 Pipes
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Monel K500 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
Mechanical Properties of Monel K500
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel K500 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
Markings On The Monel K500 Pipes
The full identification of the pipe should be continuously marked down its whole length, including :
- Nominal Pipe Size (Nominal Bore)
- Schedule (Wall Thickness)
- Specification
- Grade
- Method of Manufacture (Seamless or Welded)
- Heat Number
- Stockist’s Name or Symbol
Monel K500 Pipes Application Industries
- Aerospace Industry
- Chemical Industry
- Energy Industry
- Food Processing Industry
- Oil and Gas Industry
- Petrochemical Industry
- Pulp & Paper Industry
- Pharmaceuticals Industry
- Power Plant Industry
People Also Searched for
monel alloy K500 pipe weight chart, monel K500 pipe price list in india, alloy K500 erw pipe Stockist, asme sb165 monel K500 pipe, astm b165 alloy K500 seamless pipe, monel K500 pipe Stockists in india, weight of monel alloy K500 pipe, monel K500 seamless pipe Stockist, alloy K500 seamless pipe, monel K500 pipe price per kg in india, monel K500 pipe price list pdf, alloy K500 seamless pipe Stockist, monel K500 pipe price, seamless monel alloy K500 pipe, monel alloy K500 pipe Stockist in india, alloy K500 pipe price list, monel K500 pipes Stockist in mumbai, monel alloy K500 welded pipe Stockist, monel K500 large diameter pipes, cost of K500 monel pipe, alloy K500 pipe price per meter, monel K500 seamless pipes Stockist in india, price of monel alloy pipe K500, monel K500 pipe weight, alloy K500 pipe Stockist in mumbai, monel K500 pipe sizes, monel K500 pipe weight calculator.
Product
| Inconel 718 Pipes & Tubes |
| Inconel 718 Plates & Sheets |
| Inconel 718 Flanges |
| Inconel 718 Filler wire |
| Inconel 718 Round Bars |
| Inconel 718 Coils |
| Inconel 718 Buttweld Fitting |
| Incoloy 825 Pipes & Tubes |
| Incoloy 825 Plates & Sheets |
| Incoloy 825 Flanges |
| Incoloy 825 Filler wire |
| Incoloy 825 Round Bars |
| Incoloy 825 Coils |
| Incoloy 825 Buttweld Fitting |