MV Super Alloys, the Importer and Stockist, supplies Monel K500 Round Bars. We also have a period of experience in the industry and quality control management to attain the best products that are delivered around the world. Please get in touch with us about any questions or concerns; we are available 24 hours.
Monel K500 is nickel-copper alloys known for representing excellent properties such as accurate dimension, rugged construction and high toughness. The chemical composition of both grades is almost similar and generally hardenable due to aluminium and titanium alloys in small proportions. Monel K500 grade has a chemical composition that includes up to 63 per cent nickel, 30 per cent copper to maintain chemical properties. Up to 2% manganese and other minor components. Monel K500 has a variety of qualities. It is an age-hardenable alloy of alloy K500 with excellent tensile strength and erosion resistance, highly sought after by our customers. The mechanical strength of K500 is outstanding from “0” temperature ranges up to 480ºC. Due to the extensive corrosion resistance, their needs are generally considered across marine and chemical environments. The following grades are highly resistant from pure water to acidic or non-oxidizing environments. Monel K500 is considered difficult while machining; these alloys can be mainly machined using conventional production methods at a suitable speed. During machining, these grades quickly get hardened while producing the heat during cutting. However, K500 offers high resistance across metal removal due to their high shear strength.
Turbine and pump shafts are some of the applications for Monel K500, as are components used in petrochemical and chemical processing, valve components, oil and gas production industries, sea and marine components, and offshore industries.
Monel K500 Bright Bar Stockists, Monel Alloy K500 Rods, Monel 2.4360 Round Bars, Monel K500 Cold Finish Round Bar, ASTM B164 Monel K500 Round Bars, Monel K500 Forged Bar Importer in India.
Monel UNS N04K500 Round Bar, ASTM B164 K500 Monel Bars, Monel K500 Square Bar, Monel K500 Flat Bar, Monel K500 Hex Bar, Monel Alloy K500 Round Bar, K500 Monel Rods, Monel K500 Round Bar Stockist in Mumbai, India.
ASTM B164 Monel K500 Round Bars Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Monel K500 | 2.4360 | N04K500 | NW 4K500 | NA 13 | МНЖМц 28-2,5-1,5 | NU-30M | NiCu30Fe |
ASTM B164 Monel K500 Bars Forms in Stock
ASTM B164 Monel K500 Round Bar:
ASTM B164 is the standard specification for Monel K500 round bars. These bars are cylindrical in shape and available in various diameters. Monel K500 round bars are widely used in various industries due to their excellent corrosion resistance and high strength properties. They are commonly used in marine environments, chemical processing, and aerospace applications.
ASTM B164 Monel K500 Square Bar:
ASTM B164 Monel K500 square bars are square-shaped bars that provide excellent mechanical properties and resistance to corrosion. The square shape makes them suitable for various structural and mechanical applications, where strength and corrosion resistance are essential.
ASTM B164 Monel K500 Hollow Bar:
ASTM B164 Monel K500 hollow bars are tubes with a circular or rectangular cross-section and are known for their high strength and durability. These hollow bars are used in applications that require lightweight yet strong components, such as in the aerospace and automotive industries.
ASTM B164 Monel K500 Hex Bar:
ASTM B164 Monel K500 hex bars have a hexagonal cross-section and offer enhanced strength and stability. The hex shape allows for a better grip and makes these bars suitable for fasteners, nuts, and bolts, as well as in machinery and construction applications.
ASTM B164 Monel K500 Bright Bar:
ASTM B164 Monel K500 bright bars are polished and smooth-surfaced bars that are ideal for applications requiring a bright and lustrous finish. These bars are widely used in decorative and ornamental applications, as well as in industries where aesthetics are crucial.
ASTM B164 Monel K500 Forged Bar:
ASTM B164 Monel K500 forged bars are shaped by the process of forging, which enhances their mechanical properties and grain structure. Forged bars are known for their excellent strength and reliability and are commonly used in heavy-duty applications such as in the oil and gas, power generation, and chemical industries.
Stock Size Range and Specifications For ASTM B164 Monel K500 Round Bar
| Dimensions | ASTM, ASME and API |
| Standard Specification | ASTM B 164, B 865, ASME SB 164, SB 865 |
| Size | 6 mm to 120 mm. |
| Length | Random, Fix & Cut Length |
| Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
| Form | Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc |
| Surface | Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline |
Chemical Composition of Monel K500 Round Bars
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Monel K500 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
Mechanical Properties of Monel K500 / N04K500 / 2.4360 Round Bars
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel K500 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
Markings On The Monel K500 Round Bar
The full identification of the bars should be continuously marked down its whole length, including :
- Rating Designation
- Material Designation
- “WP” in grade symbol
- Grade
- Schedule number or nominal wall thickness
- Heat Code
- Stockist’s Name or Symbol
ASTM B164 Monel K500 Bars Application Industries
- Aerospace Industry
- Chemical Industry
- Energy Industry
- Food Processing Industry
- Oil and Gas Industry
- Petrochemical Industry
- Pulp & Paper Industry
- Pharmaceuticals Industry
- Power Plant Industry
People Also Searched for
ASME SB164 Cold Drawn Bar, EN Nicu30Fe Triangle Rod, ASME SB164 Bright Rod, ASME SB164 Threaded Rod, BS Na 13 Y Shape Bar, ASTM B164 Bright Bar, JIS NW 4K500 Hex Bar, JIS NW 4K500 Square Bar, UNS N04K500 Industrial Bar stockiest in Vietnam, BS Na 13 Rectangular Bar trader in Thailand, ASTM B164 Peeled Rod trader in Oman, ASTM B164 Threaded Rod trader in sharjah, BS Na 13 Threaded Bar Stockist in Saudi Arabia, Werkstoff Nr. 2.4360 Threaded Rod Stockist in Qatar, ASTM B164 Peeled Rod Stockist in Malaysia, ASME SB164 Half Round Bar Stockist in Philippines, Werkstoff Nr. 2.4360 Y Shape Bar Importer in Oman, ASME SB164 Industrial Rod wholesaler in Chennai, BS Na 13 Threaded Rod Trader in Ahmedabad, ASTM B164 Black Rod wholesaler in Pune, UNS N04K500 Industrial Rod Trader in Qatar, Monel K500 Flat Bar Importer in Kuwait, UNS N04K500 Rectangular Bar trader in Malaysia, ASTM B164 Threaded Rod trader in Saudi Arabia, ASME SB164 Polished Bar Stockist in Qatar, ASME SB164 Rectangular Rod stockiest in Saudi Arabia, Werkstoff Nr. 2.4360 Threaded Bar Trader in Vietnam, ASTM B164 Y Shape Rod Stockist in sharjah, Monel K500 Cold Drawn Bar trader in India, Monel K500 Black Bar wholesaler in sharjah, Monel K500 Bright Bar Stockist in Pune, Werkstoff Nr. 2.4360 Triangle Rod Stockist in sharjah, BS Na 13 Hexagonal Rod trader in Saudi Arabia, Werkstoff Nr. 2.4360 Round Rod, BS Na 13 Hex Bar, ASME SB164 Black Bar, Monel K500 Black Rod, BS Na 13 Black Rod, JIS NW 4K500 Industrial Rod, ASTM B164 Rectangular Bar, UNS N04K500 Y Shape Rod, EN Nicu30Fe Round Rod, Werkstoff Nr. 2.4360 Hexagonal Rod, JIS NW 4K500 Black Rod, ASME SB164 Bright Bar, Werkstoff Nr. 2.4360 Half Round Bar
Product
| Inconel 718 Pipes & Tubes |
| Inconel 718 Plates & Sheets |
| Inconel 718 Flanges |
| Inconel 718 Filler wire |
| Inconel 718 Round Bars |
| Inconel 718 Coils |
| Inconel 718 Buttweld Fitting |
| Incoloy 825 Pipes & Tubes |
| Incoloy 825 Plates & Sheets |
| Incoloy 825 Flanges |
| Incoloy 825 Filler wire |
| Incoloy 825 Round Bars |
| Incoloy 825 Coils |
| Incoloy 825 Buttweld Fitting |