ASTM B160 200 Nickel Bars, Nickel UNS N02200 Round Bar, Nickel 200 Square Bar, Nickel 200 Flat Bar, Nickel 200 Hex Bar, Nickel Alloy 200 Round Bar, 200 Nickel Rods, Nickel 200 Round Bar Stockist in Mumbai, India.
MV Super Alloys has been importing and Stocking high-quality Nickel 200 Round Bars. We’ve assembled some talented, qualified engineers focused on delivering the greatest quality products to customers all around the world. Because we provide 24-hour customer support, you can reach us at any time.
Nickel 200 Round bars are pure nickel-cobalt austenitic alloys with good tensile strength and good corrosion resistance against crevice, pitting and intergranular corrosions, and many other reducing environments. 200 Nickel has 99% minimum nickel proportion, and the remaining 1% consists of copper, nickel, manganese, and carbon-like elements. Nickel 200 and 200 grades show various properties in many corrosive atmospheres and acidic and alkaline environments. Nickel 200 allows hot forming at the temperature range from 870-1230ºC. In any operation, raising the temperature above 1230ºC might result in dissimilar properties. Any conventional cold methods can utilize nickel 200 Rounds Bars, and the results are about equivalent to mild steels. The power requirement in operation is high due to the high tensile limit on both grades. Nickel 200 and 200 are generally machined in the annealed condition in most possibilities. To assure optimal heat conductivity, liquid cold forming lubricants are required during machining. Both 200 and 200 have unique features that fall in the top class superior quality alloys list with enriched corrosion resistance properties that even enhanced the supply of Nickel 200 Round Bars across the world.
Nickel 200 Round Bars are used in aircraft and missile components, chemical processing, food processing equipment, marine and maritime industries, and petrochemical processing, among other uses.
Nickel 200 Bright Bar Stockists, Nickel Alloy 200 Rods, Nickel 2.4066 Round Bars, Nickel 200 Cold Finish Round Bar, ASTM B160 Nickel 200 Round Bars, Nickel 200 Forged Bar Importer in India.
ASTM B160 200 Nickel Round Bar, Nickel Alloy 200 Industrial Bars Trader, ASTM B160 Nickel 200 Hexagonal Bars, Nickel 200 Threaded Bar, Nickel 200 Polished Bars at Best Price, Nickel 200 Round Bar Stockist in India.
ASTM B160 Nickel 200 Round Bars Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Nickel 200 | 2.4066 | N02200 | NW 2200 | NA 11 | НП-2 | N-100M | Ni 99.2 |
| Nickel 200 | 2.4068 | N02200 | NW 2200 | NA 12 | НП-2 | – | LC-Ni 99 |
ASTM B160 Nickel 200 Bars Forms in Stock
ASTM B160 Nickel 200 Round Bar:
- ASTM B160 Nickel 200 round bar is a solid cylindrical bar made from nickel alloy grades 200 and 200. These round bars are manufactured according to the specifications outlined in ASTM B160, ensuring high quality and dimensional accuracy. Nickel 200 round bars offer excellent corrosion resistance and high thermal conductivity, making them suitable for various applications in industries such as chemical processing, aerospace, and marine environments.
ASTM B160 Nickel 200 Square Bar:
- ASTM B160 Nickel 200 square bar is a solid square-shaped bar made from nickel alloy grades 200 and 200. These square bars are also manufactured to meet the standards specified in ASTM B160, ensuring reliable performance. Nickel 200 square bars are used in applications requiring precise dimensions and exceptional resistance to corrosive environments.
ASTM B160 Nickel 200 Hollow Bar:
- ASTM B160 Nickel 200 hollow bar is a tubular bar with an empty interior, made from nickel alloy grades 200 and 200. These hollow bars offer reduced weight while maintaining strength, making them suitable for applications where weight reduction is essential. Nickel 200 hollow bars are used in industries such as aerospace, petrochemical, and electrical components.
ASTM B160 Nickel 200 Hex Bar:
- ASTM B160 Nickel 200 hex bar is a bar with a hexagonal cross-section made from nickel alloy grades 200 and 200. These hex bars offer superior mechanical properties and are used in various applications requiring enhanced strength and stability. Nickel 200 hex bars find use in industries such as chemical processing, electronics, and automotive.
ASTM B160 Nickel 200 Bright Bar:
- ASTM B160 Nickel 200 bright bar is a polished and smooth-surfaced bar made from nickel alloy grades 200 and 200. These bright bars undergo additional finishing processes to achieve a refined and lustrous appearance. Nickel 200 bright bars are used in decorative applications as well as in industries where a smooth surface is necessary for easy cleaning and hygiene.
ASTM B160 Nickel 200 Forged Bar:
- ASTM B160 Nickel 200 forged bar is a bar formed through the forging process, which involves compressive forces to shape the material. Forged bars offer superior strength and enhanced grain structure. Nickel 200 forged bars are used in critical applications requiring high mechanical properties, such as aerospace, oil and gas, and chemical processing.
Stock Size Range and Specifications For ASTM B160 Nickel 200 Round Bar
| Specification | EN, DIN, JIS, ASTM, BS, ASME, AISI |
| Standard Specification | ASTM B160 / ASME SB160 |
| Size | 15NB to 150NB IN |
| Diameter | 3.17mm to 350mm diameter |
| Length | 100 mm to 3000 mm Long & Above |
| Tolerance | H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients’ requirements |
| Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
| Form | Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc |
| Surface | Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline |
| Condition | Cold Drawn Polished Cold Drawn Centreless Ground & Polished |
Chemical Composition of Nickel 200 Round Bars
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Nickel 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Nickel 200 | 0.02 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
Mechanical Properties of Nickel 200 / N02200 / 2.4066 Round Bars
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Nickel 200 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
Markings On The Nickel 200 Round Bar
The full identification of the bars should be continuously marked down its whole length, including :
- Rating Designation
- Material Designation
- “WP” in grade symbol
- Grade
- Schedule number or nominal wall thickness
- Heat Code
- Stockist’s Name or Symbol
ASTM B160 Nickel 200 Bars Application Industries
- Aerospace Industry
- Chemical Industry
- Energy Industry
- Food Processing Industry
- Oil and Gas Industry
- Petrochemical Industry
- Pulp & Paper Industry
- Pharmaceuticals Industry
- Power Plant Industry
People Also Searched for
Werkstoff Nr. 2.4068 Triangle Bar dealer in India, JIS NW 2200 Hexagonal Bar Importer in Philippines, ASME SB160 Industrial Rod Stockist in Kolkata, Werkstoff Nr. 2.4068 Industrial Rod Stockist in Qatar, Nickel 200 Square Rod wholesaler in Saudi Arabia, Alloy 200 Nickel Peeled Rod Stockist in Singapore, Alloy 200 Nickel Hot Rolled Rod dealer in Qatar, Nickel 200 Triangle Rod Stockist in Coimbatore, ASTM B160 Industrial Rod Importer in Philippines, UNS N02200 Cold Drawn Bar dealer in Pune, ASTM B160 Peeled Rod stockist in Saudi Arabia, ASTM B160 Industrial Rod trader in Kuwait, ASME SB160 Rectangular Rod trader in Qatar, ASTM B160 Peeled Bar Importer in sharjah, Werkstoff Nr. 2.4068 Square Rod trader in Pune, UNS N02200 Cold Drawn Rod Stockist in Saudi Arabia, ASME SB160 Triangle Bar wholesaler in Thailand, ASTM B160 Rectangular Bar Stockist in Pune, EN Lc-Ni 99 Industrial Rod trader in Indonesia, Alloy 200 Nickel Black Rod wholesaler in Indonesia, Nickel 200 Flat Rod stockist in Mumbai, UNS N02200 Hexagonal Bar Stockist in Kolkata, ASTM B160 Industrial Rod wholesaler in Philippines, JIS NW 2200 Triangle Rod trader in Thailand, UNS N02200 Bright Bar Importer in Mumbai, Werkstoff Nr. 2.4068 Polished Bar trader in Ahmedabad, Werkstoff Nr. 2.4068 Polished Rod dealer in Coimbatore, Alloy 200 Nickel Black Rod trader in Philippines, ASTM B160 Cold Drawn Bar trader in Philippines, ASME SB160 Peeled Rod Importer in Mumbai, JIS NW 2200 Bright Rod dealer in Vietnam, Werkstoff Nr. 2.4068 Polished Bar stockist in Malaysia, Werkstoff Nr. 2.4066 Round Rod trader, Nickel 200 Flat Bar stockist, Alloy 200 Nickel Bright Rod wholesaler, ASTM B160 Triangle Bar retailer, JIS NW 200 Cold Drawn Rod retailer, ASTM B160 Cold Drawn Bar wholesaler, EN X6Crniti18-12 Bright Rod dealer, Werkstoff Nr. 2.4066 Cold Drawn Bar Importer, ASTM B160 Cold Drawn Rod dealer, ASME SB160 Black Rod trader, Nickel 200 Rectangular Rod stockist, JIS NW 200 Threaded Bar stockist, Werkstoff Nr. 2.4066 Hexagonal Bar dealer, UNS N02200 Y Shape Rod trader, EN X6Crniti18-12 Flat Bar trader, ASME SB160 Round Rod retailer, ASTM B160 Y Shape Bar Stockist
Product
| Inconel 718 Pipes & Tubes |
| Inconel 718 Plates & Sheets |
| Inconel 718 Flanges |
| Inconel 718 Filler wire |
| Inconel 718 Round Bars |
| Inconel 718 Coils |
| Inconel 718 Buttweld Fitting |
| Incoloy 825 Pipes & Tubes |
| Incoloy 825 Plates & Sheets |
| Incoloy 825 Flanges |
| Incoloy 825 Filler wire |
| Incoloy 825 Round Bars |
| Incoloy 825 Coils |
| Incoloy 825 Buttweld Fitting |