hastelloy c276 specifications

What is the Specification of the Hastelloy C276 Flange?

Hastelloy C276 flanges, critical in numerous commercial applications, are renowned for their remarkable corrosion resistance and sturdiness, making them sought-after additives. Understanding Hastelloy C276 specifications and properties is critical for choosing the correct flange in your specific wishes. MV Super Alloys, the maximum dependable Hastelloy C276 flanges supplier in Mumbai, takes satisfaction in offering an in-intensity form of flanges, which embody pipe fittings, to fulfill numerous assignment requirements. Renowned for our strength of will to tremendous reliability, we stand using the pinnacle vacation spot for the ones looking for top-notch Hastelloy C276 flanges. As a relied-on Hastelloy C276 flanges stockist and exporter, we make certain that our Hastelloy C276 flanges adhere to outstanding standards, along with the alloy C276 chemical composition.

 

Specifications of Hastelloy C276 Flanges:

Material Composition:

Hastelloy C276 flanges are stylishly composed of nickel, molybdenum, chromium, and iron, with small additions of tungsten and cobalt. This specific alloy composition imparts top-notch resistance to corrosion, oxidation, and pitting in harsh environments.

Sizes and Dimensions:

We provide Hastelloy C276 flanges in numerous sizes starting from 1/2″ to 60″ (15 NB to 1500 NB), catering to a big spectrum of assignment necessities. Additionally, we provide custom fabrication offerings to residence-specific dimensions consistent with client specs.

Types of Hastelloy c276 Flanges:

  • Slip-on Flanges: These flanges slide over the give-up of piping and are welded in the area for a steady connection.
  • Weld Neck Flanges: Featuring a tapered hub, weld neck flanges offer excessive strength and resistance to deformation beneath stress.
  • Blind Flanges: Used to seal the surrender of piping structures, blind flanges prevent the go along with the go with the go-with the flow of fluids and gases.
  • Lap Joint Flanges: Lap joint flanges are perfect for applications requiring common dismantling and assembly.
  • Threaded Flanges: Threaded flanges have characteristic inner threads for smooth installation onto threaded pipes or fittings.
  • Socket Weld Flanges: Designed for socket welding, those flanges offer greater suitable power and sturdiness.

Standards and Certifications:

Our Hastelloy C276 flanges agree to international requirements which encompass ASTM B564, ASME SB564, DIN 2.4819, and ANSI B16.5/B16.47. Additionally, every flange is observed through a Material Test Certificate (MTC), ensuring compliance with organization policies and specs.

 

Equivalent Grade of Hastelloy Alloy C276 Flanges

Standard Werkstoff Nr. UNS EN
Hastelloy C276 2.4819 N10276 NiMoCr15W

 

Alloy C276 Flanges Chemical Composition

Grade C Mn Si S Co Ni Cr Fe Mo P
Hastelloy C276 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 Max

 

Mechanical Properties of ASTM B575 Hastelloy C276 Flanges

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C276 8.89g/cm3 1370 °C (2500 °F) Psi – 1,15,000, MPa – 790 Psi – 52,000, MPa – 355 40 %

 

Uses & Applications of Hastelloy C276 Flanges

  • Chemical Processing Industry
  • Oil and Gas Industry
  • Power Generation
  • Pulp and Paper Industry
  • Waste Treatment Plants
  • Marine and Offshore
  • Other Applications

 

Final Words!

Experience exceptional reliability and overall performance in corrosive environments with Hastelloy C276 flanges, the top of pleasant and durable. As leading hastelloy c276 suppliers and exporters, MV Super Alloys presents an extensive variety of flanges meticulously crafted to satisfy hastelloy c276 specifications and stringent requirements. Our hastelloy c276 pipe fittings offer great homes, making sure reliability in numerous commercial programs. Whether you’re in Hyderabad, Gujarat, Chennai, Bangalore, Mumbai, Telangana, Rajasthan, Delhi, Punjab, Himachal Pradesh, or anywhere throughout India, rely upon MV Super Alloys as your relied-on hastelloy c276 flanges supplier in Mumbai and stockist. Explore our comprehensive product services and experience excellence in each connection. Contact us today at sales@mvsapl.com to find out the satisfaction of our hastelloy c276 flanges exporter offerings.